China GBT GH2706 wrought Fe/Ni-base superalloy and GH2706 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Alloy | GH2706 | GBT | China | wrought Fe/Ni-base superalloy |
BX9Л |
|||||
CДП1-1 |
|||||
CДП1-2 |
|||||
CДП1-3 |
|||||
CДП1-4 |
|||||
CДП1-5/CAN1-5 |
|||||
GH2135 |
|||||
GH2150 |
|||||
GH2302 |
|||||
GH2696 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Cu(%) | B(%) | Nb(%) | Al(%) | Ti(%) | Fe(%) |
---|---|---|---|---|---|---|---|---|---|---|---|---|
≤0.06 | ≤0.35 | 0.35 | 0.020 | 0.015 | 14.50-17. 50 | 39.00-44.00 | 0.300 | ≤0.006 | 2. 50-3.30 | ≤0-40 | 1.50-2.00 | Bal |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
286 (≥) | 452 (≥) | 21 | 43 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 121 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
21 | - | - | 0.12 | - | |||
685 | 424 | - | 34.3 | 131 | - | ||
537 | - | 31 | 23.2 | 411 | 342 |
Heat treated : 1879°C - 1514°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com