Romania STAS/SR 40SiNiCr250 Stainless steel and 40SiNiCr250 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Special Alloy | 40SiNiCr250 | STAS/SR | Romania | Stainless steel |
| 10AlCr80 |
|||||
| 10AlCr240 |
|||||
| 10TiAlCrNi320 |
|||||
| 12NiCr250 |
|||||
| 12SiCrNi360 |
|||||
| 12TiNiCrl80 |
|||||
| 15SiNiCr200 |
|||||
| 15SiNiCr250 |
|||||
| 20VNiMoCr120 |
|||||
| 20VNiWMoCr120 |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | W(%) | Cu(%) |
|---|---|---|---|---|---|---|---|---|---|
| 0. 30-0. 50 | 1.00-2.50 | 0. 50-1.50 | 0. 045 | 0.030 | 24.0-26.0 | 19.0-21.0 | 0. 20 | 0. 40-0.60 | 0. 30 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 826 (≥) | 423 (≥) | 13 | 22 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 434 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 44 | - | - | 0.12 | - | |||
| 267 | 364 | - | 14.3 | 441 | - | ||
| 636 | - | 11 | 33.2 | 144 | 311 |
Heat treated : 1868°C - 1521°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| 40SiNiCr250 | STAS/SR | Romania | Stainless steel |