G-X300CrMoNi15-2-1 Mould Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Mould Steel | G-X300CrMoNi15-2-1 | |||
G-X300NiMo3Mg |
|||||
0.9610 |
|||||
G-X260NiCr4-2 |
|||||
0.9620 |
|||||
G-X330NiCr4-2 |
|||||
0.9625 |
|||||
G-X300NiCrSi9-5-2 |
|||||
0.9630 |
|||||
G-X300CrMo15-3 |
|||||
0.9635 |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
2.3-3.6 | 0.2-0.8 | 0.5-1.0 | 14.0-17.0 | 0.8-1.2 | ||
Mo | Al | Cu | Nb | Ti | V | Ce |
1.8-2.2 | ||||||
N | Co | Pb | B | Other | ||
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
932 (≥) | 699 (≥) | 12 | 12 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 124 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.41 | - | |||
559 | 637 | - | 43.3 | 323 | - | ||
499 | - | 31 | 14.2 | 442 | 112 |
Heat treated : 1355°C - 1145°C