E355K2 Carbon Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Carbon Steel | E355K2 | |||
| E275 |
|||||
| 1.0225 |
|||||
| E320 |
|||||
| 1.0237 |
|||||
| E355 |
|||||
| 1.0580 |
|||||
| E370 |
|||||
| 1.0261 |
|||||
| E275K2 |
|||||
| 1.0456 |
|
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
|---|---|---|---|---|---|---|
| 0.20 | 0.50 | 0.90-1.65 | 0.035 | 0.030 | ≤ 0.30 | ≤0.50 |
| Mo | Al | Cu | Nb | Ti | V | Ce |
| ≤ 0.10 | ≥ 0.020 | ≤ 0.35 | ≤ 0.050 | ≤ 0.03 | ≤0.12 | |
| N | Co | Pb | B | Other | ||
| ≤ 0.015 | ||||||
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 622 (≥) | 659 (≥) | 32 | 43 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 144 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 22 | - | - | 0.42 | - | |||
| 777 | 978 | - | 22.3 | 244 | - | ||
| 812 | - | 12 | 21.2 | 232 | 131 |
Heat treated : 1516°C - 1658°C