E275K2 Carbon Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Carbon Steel | E275K2 | |||
E260 |
|||||
1.0220 |
|||||
E275 |
|||||
1.0225 |
|||||
E320 |
|||||
1.0237 |
|||||
E355 |
|||||
1.0580 |
|||||
E370 |
|||||
1.0261 |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.20 | 0.40 | 0.50-1.40 | 0.035 | 0.030 | ≤ 0.30 | ≤0.30 |
Mo | Al | Cu | Nb | Ti | V | Ce |
≤ 0.10 | ≥ | 0.020≤ 0.35 | ≤ 0.050 | ≤ 0.03 | ≤0.05 | |
N | Co | Pb | B | Other | ||
≤ 0.015 | ||||||
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
725 (≥) | 297 (≥) | 32 | 24 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 332 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
23 | - | - | 0.32 | - | |||
993 | 486 | - | 12.3 | 414 | - | ||
392 | - | 21 | 43.2 | 122 | 411 |
Heat treated : 1255°C - 1438°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...