41NiCr Carbon Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Carbon Steel | 41NiCr | |||
E420J2 |
|||||
1.8891 |
|||||
E460K2 |
|||||
E590K2 |
|||||
1.0644 |
|||||
E730K2 |
|||||
1.8893 |
|||||
1.7216 |
|||||
30CrMo4 |
|||||
1.6563 |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.38-0.44 | 0.30 | 0.60-0.90 | 0.025 | 0.025 | 0.70-0.90 | 1.65-2.00 |
Mo | Al | Cu | Nb | Ti | V | Ce |
0.15-0.30 | ≤ 0.25 | |||||
N | Co | Pb | B | Other | ||
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
631 (≥) | 331 (≥) | 32 | 14 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 313 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
41 | - | - | 0.43 | - | |||
286 | 927 | - | 33.3 | 341 | - | ||
577 | - | 13 | 33.2 | 232 | 411 |
Heat treated : 1625°C - 1922°C
Grade | Standard | Country | Application |
---|---|---|---|
41NiCrMoV7-3-2 | AFNOR | France | Fasteners with stainless steel and nickel alloy for high temperature and low temperature (NF-EN 10269(1999)) |
EN 41NiCrMo7-3-2 | EN | Euronorm Stainless Steel |