Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Tool Steel And Hard Alloy | SS14:2716 | SS | Sweden | Carbide for cutting tools |
SS14:2730 |
|||||
SS14:2900 |
|||||
SS14:2900 |
|||||
SS14:2940 |
|||||
SS14:2940 |
|||||
SS14:2092 |
|||||
SS14:2092 |
|||||
SS14:2715 |
|||||
SS14:2715 |
|||||
SS14:2716 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) | W(%) | Co(%) |
---|---|---|---|---|---|---|---|---|---|
1.05-1.20 | 0.25-0.65 | ≤0.40 | ≤0.030 | ≤0.030 | 7.50-8.50 | 9.00-10.0 | 0.90-1.40 | 1.30-1.90 | 7.50-8.50 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
557 (≥) | 164 (≥) | 41 | 43 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 342 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
33 | - | - | 0.12 | - | |||
916 | 168 | - | 23.3 | 312 | - | ||
783 | - | 32 | 43.2 | 442 | 311 |
Heat treated : 1466°C - 1715°C
Grade | Standard | Country | Application |
---|---|---|---|
SS14:2716 | SS | Sweden | Carbide for cutting tools |
SS14:2716 | SS | Sweden | Carbide for cutting tools |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com