| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) |
|---|---|---|---|---|---|---|---|
| 0.32-0.42 | 0.80-1.20 | Max 0.50 | Max 0.030 | Max 0.020 | 4.50-5.50 | 1.00-1.50 | 0.30-0.50 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 554 (≥) | 671 (≥) | 42 | 44 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 121 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 34 | - | - | 0.34 | - | |||
| 622 | 784 | - | 21.3 | 434 | - | ||
| 881 | - | 24 | 42.2 | 134 | 433 |
Heat treated : 1776°C - 1787°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| SKD6 | JIS | Japan | Hot-work die steel |
| SKD61 | JIS | Japan | Hot-work die steel |
| SKD62 | JIS | Japan | Hot-work die steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com