France AFNOR 1.4590 Ferritic and 1.4590 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | 1.4590 | AFNOR | France | Ferritic |
1.4521 |
|||||
X2CiTi17 |
|||||
1.4520 |
|||||
X2CrMoTi17-1 |
|||||
1.4513 |
|||||
X6CrN17-1 |
|||||
1.4017 |
|||||
X6CrMoNb17-1 |
|||||
1.4526 |
|||||
X2CrNbZr17 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Nb(%) | Other(%) |
---|---|---|---|---|---|---|---|
Max 0.030 | Max 1.00 | Max 1.00 | Max 0.040 | Max 0.015 | 16.00-17.50 | 0.35-0.55 | Zr 7x(C+N)+0.15 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
989 (≥) | 118 (≥) | 31 | 32 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 111 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
13 | - | - | 0.33 | - | |||
966 | 571 | - | 13.3 | 344 | - | ||
214 | - | 22 | 41.2 | 113 | 222 |
Heat treated : 1249°C - 1733°C