USA SAE SAE J 437 (1970), SAE J 438 (1970), W209 Special Tool Die Steels Tool and die steels and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Tool Die Steels | W209 Special | SAE | USA | Tool and die steels | 
| C | Si | Mn | Cr | V | 
|---|---|---|---|---|
| 0.85 -0.95 | 0.10 -0.40 | 0.10 -0.40 | ≤ ≥ | 0.15 -0.35 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 193 (≥) | 315 (≥) | 12 | 44 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 444 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.21 | - | |||
| 991 | 833 | - | 21.3 | 434 | - | ||
| 449 | - | 31 | 22.2 | 123 | 132 | 
Heat treated : 1759°C - 1232°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| AISI W209 Commercial | |||
| SAE W209 Commercial | |||
| ASTM W209 Standard | |||
| ASTM W209 Extra | |||
| ASTM W209 Special | |||
| UNS W20918 | 
| SAE J 437 (1970) | Selection and heat treatment of tool and die steels | SAE-J-437-(1970).pdf | 
| SAE J 438 (1970) | Tool and die steels | SAE-J-438-(1970).pdf | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com