Available 24/7 at contact@steel-grades.com

PSL2 Grade X56Q

Description

France AFNOR NF EN ISO 3183, PSL2 Grade X56Q Superalloys Petroleum and natural gas industries-Steel pipe for pipeline transportation systems(ISO 3183:2012) and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

Datasheet for: Steel Grades:Superalloys: PSL2 Grade X56Q
Category Class Grade Type Standard Country Application
Steel GradesSuperalloys PSL2 Grade X56Q Austenite AFNOR France Petroleum and natural gas industries-Steel pipe for pipeline transportation systems(ISO 3183:2012)

Chemical composition(mass fraction)(wt.%) of the PSL2 Grade X56Q

CE Pcm C Mn P S Si Ni Cr Mo Cu V Ti Nb Nb+Ti+V CEV
≤0.2500 ≤0.1800 ≤1.5000 ≤0.0250 ≤0.0150 ≤0.4500 ≤0.3000 ≤0.3000 ≤0.1500 ≤0.50 ≤0.0700 ≤0.0400 ≤0.0500 ≤0.1500 ≤0.43

Mechanical Properties of steel grade PSL2 Grade X56Q

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
261 (≥) 622 (≥) 14 22 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical Properties of steel grade PSL2 Grade X56Q

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
32 - -     0.31 -  
529 563 - 34.3 433   -  
459 - 43 43.2   341 221

Heat Treatment of steel grade PSL2 Grade X56Q

Heat treated : 1995°C - 1939°C

Technological Curves of steel grade PSL2 Grade X56Q

Relevant standard of PSL2 Grade X56Q

NF EN ISO 3183 Petroleum and natural gas industries-Steel pipe for pipeline transportation systems(ISO 3183:2012) NF-EN-ISO-3183.pdf

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this PSL2 Grade X56Q?
  • List your company on S&G now? Join
  • Non-paying users only
Top