NIMONIC® alloy 105

Description

USA SMC SMC-081, NIMONIC® alloy 105 Superalloys NIMONIC® alloy 105 and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

Datasheet for: Steel Grades:Superalloys: NIMONIC® alloy 105
Category Class Grade Standard Country Application
Steel GradesSuperalloys NIMONIC® alloy 105 SMC USA NIMONIC® alloy 105

Chemical composition(mass fraction)(wt.%) of the NIMONIC® alloy 105

C Si Cu Fe Mn Cr Ti Al Co Mo Pb S B Zr Ni
≤0.17 ≤1.00 ≤0.20 ≤1.00 ≤1.00 14.00 -15.70 0.90 -1.50 4.50 -4.90 18.00 -22.00 4.50 -5.50 ≤0.0015 ≤0.0100 0.0030 -0.0100 ≤0.1500 ≤Balance

Mechanical Properties of steel grade NIMONIC® alloy 105

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
499 (≥) 957 (≥) 34 41 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 124

Physical Properties of steel grade NIMONIC® alloy 105

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
14 - -     0.43 -  
871 815 - 22.3 321   -  
431 - 12 14.2   324 331

Heat Treatment of steel grade NIMONIC® alloy 105

Heat treated : 1854°C - 1266°C

Technological Curves of steel grade NIMONIC® alloy 105

Cross Reference Table (Equivalent Grade) of NIMONIC® alloy 105

Relevant standard of NIMONIC® alloy 105

SMC-081 NIMONIC® alloy 105 (W. Nr. 2.4634) SMC-081.pdf

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this NIMONIC® alloy 105?
  • List your company on S&G now? Join
  • Non-paying users only
Top