USA SMC SMC-081, NIMONIC® alloy 105 Superalloys NIMONIC® alloy 105 and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Superalloys | NIMONIC® alloy 105 | SMC | USA | NIMONIC® alloy 105 |
| C | Si | Cu | Fe | Mn | Cr | Ti | Al | Co | Mo | Pb | S | B | Zr | Ni |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| ≤0.17 | ≤1.00 | ≤0.20 | ≤1.00 | ≤1.00 | 14.00 -15.70 | 0.90 -1.50 | 4.50 -4.90 | 18.00 -22.00 | 4.50 -5.50 | ≤0.0015 | ≤0.0100 | 0.0030 -0.0100 | ≤0.1500 | ≤Balance |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 918 (≥) | 421 (≥) | 44 | 11 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 241 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.11 | - | |||
| 541 | 932 | - | 13.3 | 433 | - | ||
| 628 | - | 44 | 34.2 | 414 | 422 |
Heat treated : 1968°C - 1311°C
| SMC-081 | NIMONIC® alloy 105 (W. Nr. 2.4634) | SMC-081.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com