USA SAE Rod, Bar, Pipe, Tube, Plate, Sheet, Strip, Fittings, Forgings, Wire, Other/Similar Specs, Nickel Alloy 201 Superalloys Wrought nickel and nickel-related alloys and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Superalloys | Nickel Alloy 201 | SAE | USA | Wrought nickel and nickel-related alloys |
| C | Cu | Fe | Mn | C | Si | S |
|---|---|---|---|---|---|---|
| 99.0 - ≥ | ≤0.25 | ≤0.40 | ≤0.35 | ≤0.02 | ≤0.35 | ≤0.01 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 526 (≥) | 793 (≥) | 41 | 31 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 313 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 42 | - | - | 0.33 | - | |||
| 649 | 237 | - | 13.3 | 332 | - | ||
| 531 | - | 42 | 11.2 | 114 | 414 |
Heat treated : 1115°C - 1853°C
| Rod | ASTM B 160, ASME SB 160, DIN 17752, ISO 9723 | Rod.pdf |
| Bar | ASTM B 160, ASME SB 160, DIN 17752, ISO 9723 | Bar.pdf |
| Pipe | ASTM B 161, ASME SB161, ASTM B 163, ASME SB 163, ASTM B 725, ASME SB 725, ASTM B 730, ASME SB 730, ASTM B 751, ASME B 751, ASTM B775, ASME SB 775, ASTM B 829, ASME SB 829 DIN 17751, ISO 6207 | Pipe.pdf |
| Tube | ASTM B 161, ASME SB161, ASTM B 163, ASME SB 163, ASTM B 725, ASME SB 725, ASTM B 730, ASME SB 730, ASTM B 751, ASME B 751, ASTM B775, ASME SB 775, ASTM B 829, ASME SB 829 DIN 17751, ISO 6207 | Tube.pdf |
| Plate | ASTM B 162, ASME SB 162, DIN 17750, ISO 6208 | Plate.pdf |
| Sheet | ASTM B 162, ASME SB 162, DIN 17750, ISO 6208 | Sheet.pdf |
| Strip | ASTM B 162, ASME SB 162, DIN 17750, ISO 6208 | Strip.pdf |
| Fittings | ASTM B 366, ASME SB 366 | Fittings.pdf |
| Forgings | ASTM B 546, ASME SB 564, ISO 9725, DIN 17754 | Forgings.pdf |
| Wire | DIN 17753, ISO 9724 | Wire.pdf |
| Other/Similar Specs | Other/Similar Specs | Other-Similar-Specs.pdf |