Available 24/7 at contact@steel-grades.com

F1091 R30605

Description

USA ASTM F 1091 (2012), F1091 R30605 Superalloys Standard Specification for Wrought Cobalt-20Chromium-15Tungsten-10Nickel Alloy Surgical Fixation Wire (UNS R30605) and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

Datasheet for: Steel Grades:Superalloys: F1091 R30605
Category Class Grade Standard Country Application
Steel GradesSuperalloys F1091 R30605 ASTM USA Standard Specification for Wrought Cobalt-20Chromium-15Tungsten-10Nickel Alloy Surgical Fixation Wire (UNS R30605)

Chemical composition(mass fraction)(wt.%) of the F1091 R30605

C P Mn S Si Cr Ni Co Fe W
0.05 -0.15 ≤0.40 1.00 -2.00 ≤0.03 ≤0.40 19.00 -21.00 9.00 -11.00 ≤Bal ≤3.0 14.00 -16.00

Mechanical Properties of steel grade F1091 R30605

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
286 (≥) 161 (≥) 22 13 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical Properties of steel grade F1091 R30605

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
21 - -     0.22 -  
156 631 - 13.3 243   -  
967 - 34 22.2   322 412

Heat Treatment of steel grade F1091 R30605

Heat treated : 1716°C - 1883°C

Technological Curves of steel grade F1091 R30605

Cross Reference Table (Equivalent Grade) of F1091 R30605

Grade Standard Country Application
HS-25
R30605
UNS R30605
UNS R30605

Relevant standard of F1091 R30605

F 1091 (2012) Standard Specification for Wrought Cobalt-20Chromium-15Tungsten-10Nickel Alloy Surgical Fixation Wire (UNS R30605) F-1091-(2012).pdf

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this F1091 R30605?
  • List your company on S&G now? Join
  • Non-paying users only
Top