Chemical composition(mass fraction)(wt.%) of the N07750

C Mn Si S P Cu Fe Co Nb Cr Ni Al Ti
≤0.08 ≤1.0 ≤0.5 ≤0.01 ≤0.015 ≤0.5 5.0 -9.0 ≤1.0 0.70 -1.20 14.0 -17.0 70 - ≥ 0.40 -1.00 2.25 -2.75

Mechanical Properties of steel grade N07750

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
341 (≥) 836 (≥) 22 21 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

Physical Properties of steel grade N07750

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
13 - -     0.11 -  
368 325 - 22.3 132   -  
782 - 34 23.2   312 433

Heat Treatment of steel grade N07750

Heat treated : 1236°C - 1844°C

Technological Curves of steel grade N07750

Cross Reference Table (Equivalent Grade) of N07750


Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this N07750?
  • List your company on S&G now? Join
  • Non-paying users only
Top