USA ASTM B 637 (2012), B 637 N07718 Superalloys Precipitation-Hardening and Cold Worked Nickel Alloy Bars, Forgings, and Forging Stock for Moderate or High Temperature Service and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Superalloys | B 637 N07718 | ASTM | USA | Precipitation-Hardening and Cold Worked Nickel Alloy Bars, Forgings, and Forging Stock for Moderate or High Temperature Service |
| C | Cr | Mo | Ni | Al | Nb | Fe | Si | Mn | P | S | B |
|---|---|---|---|---|---|---|---|---|---|---|---|
| ≤0.03 | 17.0 -21.0 | 2.80 -3.30 | 50.0 -55.0 | 0.20 -0.60 | 4.75 -5.50 | ≤Bal | ≤0.35 | ≤0.35 | ≤0.015 | ≤0.015 | ≤0.006 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 588 (≥) | 611 (≥) | 44 | 31 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 331 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 12 | - | - | 0.21 | - | |||
| 416 | 942 | - | 41.3 | 211 | - | ||
| 495 | - | 32 | 33.2 | 122 | 344 |
Heat treated : 1423°C - 1647°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| NiCr19Fe19Nb5Mo3 |
| B 637 (2012) | Precipitation-Hardening and Cold Worked Nickel Alloy Bars, Forgings, and Forging Stock for Moderate or High Temperature Service | B-637-(2012).pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com