USA UNS ASTM B409, ASTM B514, ASTM B515, Incoloy 800 Superalloys Equipment used in the manufacture of resistance to stress corrosion cracking and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Superalloys | Incoloy 800 | UNS | USA | Equipment used in the manufacture of resistance to stress corrosion cracking |
| C | Si | Mn | P | S | Cr | Ni | Fe |
|---|---|---|---|---|---|---|---|
| ≤0.10 | ≤1.00 | ≤1.50 | ≤0.030 | ≤0.015 | 19.00 -23.00 | 30.00 -35.00 | ≤Bal |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 676 (≥) | 566 (≥) | 41 | 42 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 122 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 42 | - | - | 0.34 | - | |||
| 627 | 685 | - | 21.3 | 411 | - | ||
| 928 | - | 43 | 13.2 | 233 | 214 |
Heat treated : 1143°C - 1538°C
| ASTM B409 | Stainless steel hot rolled steel plate | ASTM-B409.pdf |
| ASTM B514 | Stainless steel cold rolled steel sheet | ASTM-B514.pdf |
| ASTM B515 | Stainless steel/acid steel cold rolling belt | ASTM-B515.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...