MONEL ALLOY 400

Description

USA UNS UNS N04400, BS 3072 – 3076 (NA13), SAE AMS 4544, 4574, 4675, 4730, 4731, 7233, DIN 17743, 17750 – 17754, ASTM B 127, B 163 – B 165,B 366, B 564, B 725, B 730,B 751, B 775, B 829, ASME SB-127, SB-163 – SB-165,SB-366, SB-564, SB-725,SB-730, SB-751, SB-775,SB-829, MONEL ALLOY 400 Superalloys Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire. and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

Datasheet for: Steel Grades:Superalloys: MONEL ALLOY 400
Category Class Grade Standard Country Application
Steel GradesSuperalloys MONEL ALLOY 400 UNS USA Pipe, tube, sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.

Chemical composition(mass fraction)(wt.%) of the MONEL ALLOY 400

Ni Mn S Cu C Fe Si
63.00 - ≥ ≤2.00 ≤0.50 28.00 -34.00 ≤0.30 ≤2.50 ≤0.024

Mechanical Properties of steel grade MONEL ALLOY 400

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
832 (≥) 925 (≥) 22 22 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical Properties of steel grade MONEL ALLOY 400

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
14 - -     0.11 -  
788 988 - 31.3 211   -  
636 - 33 42.2   412 141

Heat Treatment of steel grade MONEL ALLOY 400

Heat treated : 1554°C - 1421°C

Technological Curves of steel grade MONEL ALLOY 400

Relevant standard of MONEL ALLOY 400


Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this MONEL ALLOY 400?
  • List your company on S&G now? Join
  • Non-paying users only
Top