Description

China GB GB/T 14992 (2005), GH3652 Superalloys Classification and designation for superalloys and high temperature intermetallic materials and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

Datasheet for: Steel Grades:Superalloys: GH3652
Category Class Grade Standard Country Application
Steel GradesSuperalloys GH3652 GB China Classification and designation for superalloys and high temperature intermetallic materials

Chemical composition(mass fraction)(wt.%) of the GH3652

C Cr Ni Al Fe Ce Si Mn P S
≤0.10 26.50 -28.50 ≤Balance 2.80 -3.50 ≤1.00 ≤0.030 ≤0.80 ≤0.30 ≤0.020 ≤0.020

Mechanical Properties of steel grade GH3652

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
486 (≥) 212 (≥) 24 44 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical Properties of steel grade GH3652

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
34 - -     0.34 -  
473 367 - 13.3 343   -  
132 - 32 41.2   121 243

Heat Treatment of steel grade GH3652

Heat treated : 1569°C - 1376°C

Technological Curves of steel grade GH3652

Relevant standard of GH3652

GB/T 14992 (2005) Classification and designation for superalloys and high temperature intermetallic materials GB-T-14992-(2005).pdf

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this GH3652?
  • List your company on S&G now? Join
  • Non-paying users only
Top