Available 24/7 at contact@steel-grades.com

Description

China GB GH4738 Superalloys Nickel-base superalloy and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

Datasheet for: Steel Grades:Superalloys: GH4738
Category Class Grade Standard Country Application
Steel GradesSuperalloys GH4738 GB China Nickel-base superalloy

Chemical composition(mass fraction)(wt.%) of the GH4738

C Cr Mo Ni Co Al Ti B Fe Zr
0.03 -0.10 18.0 -21.0 3.5 -5.0 ≤Remainder 12.0 -15.0 1.2 -1.6 2.75 -3.25 0.003 -0.01 ≤2.0 0.02 -0.08

Mechanical Properties of steel grade GH4738

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
318 (≥) 294 (≥) 44 21 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical Properties of steel grade GH4738

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
11 - -     0.13 -  
643 576 - 34.3 242   -  
472 - 43 31.2   333 222

Heat Treatment of steel grade GH4738

Heat treated : 1589°C - 1256°C

Technological Curves of steel grade GH4738

Cross Reference Table (Equivalent Grade) of GH4738

Grade Standard Country Application
GH4738
GH4738

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this GH4738?
  • List your company on S&G now? Join
  • Non-paying users only
Top