China GB GH4141 Superalloys Iron-based superalloy and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.

Datasheet for: Steel Grades:Superalloys: GH4141
Category Class Grade Standard Country Application
Steel GradesSuperalloys GH4141 GB China Iron-based superalloy

Chemical composition(mass fraction)(wt.%) of the GH4141

C Cr Mo Ni Co Al Nb Ti B Fe
0.06 -0.12 18.0 -20.0 9.0 -10.5 ≤Remainder 10.0 -12.0 1.4 -2.0 2.5 -3.9 2.9 -3.5 0.003 -0.01 ≤0.5

Mechanical Properties of steel grade GH4141

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
855 (≥) 884 (≥) 22 42 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical Properties of steel grade GH4141

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
22 - -     0.14 -  
878 259 - 42.3 341   -  
895 - 14 33.2   322 123

Heat Treatment of steel grade GH4141

Heat treated : 1626°C - 1466°C

Technological Curves of steel grade GH4141

Cross Reference Table (Equivalent Grade) of GH4141

Grade Standard Country Application
GH4141
GH4141

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this GH4141?
  • List your company on S&G now? Join
  • Non-paying users only
Top