China GB GH3170 Superalloys Iron-based superalloy and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Superalloys | GH3170 | GB | China | Iron-based superalloy |
| C | Cr | Ni | Co | W | Al | B | Zr | La |
|---|---|---|---|---|---|---|---|---|
| ≤0.06 | 18.0 -22.0 | ≤Remainder | 15.0 -22.0 | 18.0 -21.0 | ≤0.5 | ≤0.005 | 0.1 -0.2 | 0.1 -0.3 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 535 (≥) | 515 (≥) | 44 | 34 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 322 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.13 | - | |||
| 866 | 617 | - | 33.3 | 312 | - | ||
| 411 | - | 14 | 14.2 | 331 | 312 |
Heat treated : 1816°C - 1987°C