China GB GH1167 Superalloys Iron-based superalloy and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Superalloys | GH1167 | GB | China | Iron-based superalloy |
| C | Cr | Mo | Ni | W | Al | Ti | B | Fe | Mn | Si | Ce | Zr |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| ≤0.08 | 13.0 -16.0 | 1.5 -2.5 | 36.0 -40.0 | 5.0 -6.5 | 1.4 -2.0 | 2.6 -3.4 | ≤0.01 | ≤Remainder | ≤0.5 | ≤0.5 | ≤0.02 | ≤0.05 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 483 (≥) | 174 (≥) | 11 | 22 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 142 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.12 | - | |||
| 762 | 268 | - | 13.3 | 412 | - | ||
| 563 | - | 44 | 23.2 | 143 | 131 |
Heat treated : 1577°C - 1716°C