USA SAE A 478 (2008) , A 478 S30940 Specialsteel Chromium-Nickel Stainless Steel Weaving and Knitting Wire and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | A 478 S30940 | Austenite | SAE | USA | Chromium-Nickel Stainless Steel Weaving and Knitting Wire |
C | Si | Mn | P | S | Cr | Ni | Nb+Ta |
---|---|---|---|---|---|---|---|
≤0.08 | ≤1.00 | ≤2.00 | ≤0.04 | ≤0.03 | 22.0 -24.0 | 12.0 -16.0 | ≤1.10 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
926 (≥) | 376 (≥) | 43 | 24 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 423 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
31 | - | - | 0.23 | - | |||
977 | 244 | - | 22.3 | 344 | - | ||
578 | - | 31 | 24.2 | 311 | 132 |
Heat treated : 1286°C - 1928°C
A 478 (2008) | Chromium-Nickel Stainless Steel Weaving and Knitting Wire | A-478--(2008)-.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com