USA AMS SA-965/SA-965M , SA-965 S30909 Specialsteel Specification for Steel Forgings, Austenitic, for Pressure and High Temperature Parts and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | SA-965 S30909 | Austenite | AMS | USA | Specification for Steel Forgings, Austenitic, for Pressure and High Temperature Parts |
C | Si | Mn | P | S | Cr | Ni |
---|---|---|---|---|---|---|
≤0.08 | ≤0.75 | ≤2.00 | ≤0.045 | ≤0.030 | 22.0 -24.0 | 12.0 -15.0 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
738 (≥) | 177 (≥) | 21 | 44 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 314 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
41 | - | - | 0.33 | - | |||
995 | 661 | - | 32.3 | 134 | - | ||
596 | - | 21 | 41.2 | 323 | 343 |
Heat treated : 1784°C - 1979°C
Grade | Standard | Country | Application |
---|---|---|---|
309HD | |||
309HCb | |||
309H | |||
309HCb | |||
TP309H | |||
TP309HCb | |||
TP309H | |||
TP309HCb | |||
TP309H | |||
TP309HCb | |||
S30909 | |||
S30909 | |||
S30909 | |||
S30909 | |||
S30909 |
SA-965/SA-965M | Specification for Steel Forgings, Austenitic, for Pressure and High Temperature Parts | SA-965-SA-965M-.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com