USA SAE A 814/A 814M , A 814 Grade TP 309 Specialsteel Cold-Worked Welded Austenitic Stainless Steel Pipe and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | A 814 Grade TP 309 | Austenite | SAE | USA | Cold-Worked Welded Austenitic Stainless Steel Pipe |
C | Si | Mn | P | S | Cr | Ni |
---|---|---|---|---|---|---|
≤0.20 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 22.0 -24.0 | 12.0 -15.0 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
272 (≥) | 614 (≥) | 11 | 14 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 433 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
33 | - | - | 0.12 | - | |||
222 | 541 | - | 23.3 | 143 | - | ||
939 | - | 21 | 43.2 | 134 | 444 |
Heat treated : 1113°C - 1949°C
Grade | Standard | Country | Application |
---|---|---|---|
1.2309 | |||
1.4309 | |||
1.6309 | |||
1.6309 | |||
1.4309 | |||
309 | |||
S30900 | |||
309S | |||
S30908 | |||
309HD | |||
S30909 | |||
309Cb | |||
S30940 | |||
309HCb | |||
S30941 | |||
309 | |||
S30900 | |||
S30908 | |||
309S | |||
S30909 |
A 814/A 814M | Cold-Worked Welded Austenitic Stainless Steel Pipe | A-814-A-814M-.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...