USA SAE A 492 (2009) , A 492 S30500 Specialsteel Stainless Steel Rope Wire and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Type | Standard | Country | Application |
|---|---|---|---|---|---|---|
| Steel Grades | Specialsteel | A 492 S30500 | Austenite | SAE | USA | Stainless Steel Rope Wire |
| C | Si | Mn | P | S | Cr | Ni |
|---|---|---|---|---|---|---|
| ≤0.12 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.030 | 17.0 -19.0 | 10.5 -13.0 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 417 (≥) | 495 (≥) | 32 | 33 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 312 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 31 | - | - | 0.11 | - | |||
| 173 | 451 | - | 31.3 | 132 | - | ||
| 751 | - | 14 | 11.2 | 343 | 233 |
Heat treated : 1162°C - 1412°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| 1.4305 | |||
| 1.4305 | |||
| 1.2305 | |||
| 305 | |||
| S30500 | |||
| S30500 | |||
| 305 | |||
| TP305 | |||
| S30500 | |||
| TP305 | |||
| S30500 | |||
| MT305 | |||
| MT-305 | |||
| 305 | |||
| S30500 | |||
| AMS 6305A | |||
| UNS T72305 | |||
| UNS W50305 | |||
| UNS S30556 | |||
| UNS K30560 |
| A 492 (2009) | Stainless Steel Rope Wire | A-492--(2009)--.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...