C | Si | Mn | P | S | Cr | Ni |
---|---|---|---|---|---|---|
≤0.12 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.030 | 17.0 -19.0 | 10.5 -13.0 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
711 (≥) | 793 (≥) | 43 | 44 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 341 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
22 | - | - | 0.34 | - | |||
947 | 183 | - | 44.3 | 112 | - | ||
391 | - | 12 | 23.2 | 241 | 324 |
Heat treated : 1239°C - 1612°C
Grade | Standard | Country | Application |
---|---|---|---|
1.4305 | |||
1.4305 | |||
1.2305 | |||
305 | |||
S30500 | |||
S30500 | |||
305 | |||
TP305 | |||
S30500 | |||
TP305 | |||
S30500 | |||
MT305 | |||
MT-305 | |||
305 | |||
S30500 | |||
AMS 6305A | |||
UNS T72305 | |||
UNS W50305 | |||
UNS S30556 | |||
UNS K30560 |
A 478 (2008) | Chromium-Nickel Stainless Steel Weaving and Knitting Wire | A-478--(2008)---.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com