USA SAE A 814/A 814M (2008) , A 814 Grade TP 304N Specialsteel Cold-Worked Welded Austenitic Stainless Steel Pipe and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | A 814 Grade TP 304N | Austenite | SAE | USA | Cold-Worked Welded Austenitic Stainless Steel Pipe |
C | Si | Mn | P | S | Cr | Ni | N |
---|---|---|---|---|---|---|---|
≤0.08 | ≤0.75 | ≤2.00 | ≤0.045 | ≤0.03 | 18.0 -20.0 | 8.00 -10.5 | 0.10 -0.16 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
371 (≥) | 679 (≥) | 11 | 43 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 312 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
14 | - | - | 0.32 | - | |||
376 | 389 | - | 41.3 | 433 | - | ||
478 | - | 34 | 12.2 | 142 | 433 |
Heat treated : 1767°C - 1195°C
Grade | Standard | Country | Application |
---|---|---|---|
304N | |||
304N | |||
TP304N | |||
TP304N | |||
TP304N | |||
TP304N | |||
SUS304N1 | |||
SUS304N2 | |||
SUS304N2A | |||
SUS304N2A | |||
SUS304N2A | |||
SUS304N2 | |||
SUS304N1 | |||
304N(S30451) | |||
SUS304N2A | |||
SUS304N2A |
A 814/A 814M (2008) | Cold-Worked Welded Austenitic Stainless Steel Pipe | A-814-A-814M--(2008)-.pdf |