China CNS G3067, G3077, G3076, CNS 317 Specialsteel Stainless steel wire rods and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | CNS 317 | Austenite | CNS | China | Stainless steel wire rods |
C | Si | Mn | P | S | Ni | Cr | Mo |
---|---|---|---|---|---|---|---|
≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.030 | 11.00 -15.00 | 18.00 -20.00 | 3.00 -4.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
521 (≥) | 942 (≥) | 14 | 32 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 232 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
32 | - | - | 0.22 | - | |||
628 | 315 | - | 34.3 | 331 | - | ||
522 | - | 43 | 22.2 | 213 | 324 |
Heat treated : 1593°C - 1917°C
Grade | Standard | Country | Application |
---|---|---|---|
1.4317 | |||
1.4317 | |||
1.4317 | |||
317 | |||
S31700 | |||
317L | |||
S31703 | |||
317LM | |||
S31725 | |||
317LMN | |||
S31726 | |||
S31727 | |||
317LN | |||
S31753 | |||
317LM | |||
317L4 | |||
S31700 | |||
317 | |||
S31703 | |||
317L |
G3067 | Stainless steel bars | G3067.pdf |
G3077 | Stainless steel wire rods | G3077.pdf |
G3076 | Stainless steel wires | G3076.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com