China CNS G3067, G3077, G3076, CNS 316 Specialsteel Stainless steel wire rods and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | CNS 316 | Austenite | CNS | China | Stainless steel wire rods |
C | Si | Mn | P | S | Ni | Cr | Mo |
---|---|---|---|---|---|---|---|
≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.030 | 10.00 -14.00 | 16.00 -18.00 | 2.00 -3.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
455 (≥) | 531 (≥) | 31 | 41 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 232 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
34 | - | - | 0.31 | - | |||
615 | 964 | - | 43.3 | 232 | - | ||
574 | - | 22 | 42.2 | 344 | 443 |
Heat treated : 1942°C - 1977°C
Grade | Standard | Country | Application |
---|---|---|---|
1.2316 | |||
1.4316 | |||
1.4316 | |||
316 | |||
S31600 | |||
316L | |||
S31603 | |||
316H | |||
S31609 | |||
316Ti | |||
S31635 | |||
316Cb | |||
S31640 | |||
316N | |||
S31651 | |||
316LN | |||
S31653 | |||
316LHN | |||
S31654 | |||
316L |
G3067 | Stainless steel bars | G3067.pdf |
G3077 | Stainless steel wire rods | G3077.pdf |
G3076 | Stainless steel wires | G3076.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...