China CNS G3067, G3077, CNS 302 Specialsteel Stainless steel wire rods and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | CNS 302 | Austenite | CNS | China | Stainless steel wire rods |
C | Si | Mn | P | S | Ni | Cr | Mo |
---|---|---|---|---|---|---|---|
≤0.15 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.030 | 8.00 -10.00 | 17.00 -19.00 | ≤ ≥ |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
972 (≥) | 568 (≥) | 41 | 42 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 224 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
21 | - | - | 0.34 | - | |||
235 | 728 | - | 13.3 | 434 | - | ||
464 | - | 22 | 22.2 | 334 | 211 |
Heat treated : 1564°C - 1526°C
Grade | Standard | Country | Application |
---|---|---|---|
1.3302 | |||
1.0302 | |||
1.4302 | |||
1.4302 | |||
302 | |||
S30200 | |||
302B | |||
S30215 | |||
S43020 | |||
S43023 | |||
T11302 | |||
302HQ-FM | |||
Custom Fol 302 HQ | |||
MAR-M 302 | |||
302B | |||
S30215 | |||
S30200 | |||
302 | |||
S30245 | |||
S43020 |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com