Korea KS D 3757 (2003), NCF825TB Specialsteel Seamless nickel-chromium-iron alloy heat exchanger tubes and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Specialsteel | NCF825TB | KS | Korea | Seamless nickel-chromium-iron alloy heat exchanger tubes |
C | Si | Mn | P | S | Cr | Ni | Cu | Al | Ti | Fe | Mo |
---|---|---|---|---|---|---|---|---|---|---|---|
≤0.05 | ≤0.50 | ≤1.00 | ≤0.030 | ≤0.015 | 19.50 -23.00 | 38.00 -46.00 | 1.50 -3.50 | ≤0.20 | 0.60 -1.20 | ≤remaining | 2.50 -3.50 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
267 (≥) | 347 (≥) | 33 | 11 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 234 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
21 | - | - | 0.13 | - | |||
192 | 458 | - | 14.3 | 412 | - | ||
971 | - | 42 | 44.2 | 421 | 443 |
Heat treated : 1563°C - 1943°C
Grade | Standard | Country | Application |
---|---|---|---|
NCF825 | |||
NCF825 TP | |||
NCF825 TB | |||
NCF825 TB | |||
NCF825 TP | |||
NCF825 | |||
NCF825 | |||
NCF825 | |||
NCF825TB | |||
NCF825TB | |||
NCF825TP | |||
NCF825TP | |||
NCF825 | |||
NCF825 |
D 3757 (2003) | Seamless nickel-chromium-iron alloy heat exchanger tubes | D-3757-(2003).pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com