Korea KS D 3758 (2003), NCF800HTP Specialsteel Seamless nickel-chromium-iron alloy pipes and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Specialsteel | NCF800HTP | KS | Korea | Seamless nickel-chromium-iron alloy pipes |
C | Si | Mn | P | S | Cr | Ni | Cu | Al | Ti | Fe |
---|---|---|---|---|---|---|---|---|---|---|
0.05 -0.10 | ≤1.00 | ≤1.50 | ≤0.030 | ≤0.015 | 19.00 -23.00 | 30.00 -35.00 | ≤0.75 | 0.15 -0.60 | 0.15 -0.60 | ≤remaining |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
476 (≥) | 612 (≥) | 34 | 42 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 341 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
13 | - | - | 0.13 | - | |||
539 | 739 | - | 44.3 | 213 | - | ||
485 | - | 42 | 31.2 | 244 | 331 |
Heat treated : 1411°C - 1626°C
Grade | Standard | Country | Application |
---|---|---|---|
NCF800H | |||
NCF800H TP | |||
NCF800H TB | |||
NCF800H TB | |||
NCF800H TP | |||
NCF800H | |||
NCF800H | |||
NCF800H | |||
NCF800HTB | |||
NCF800HTB | |||
NCF800HTP | |||
NCF800HTP | |||
SS14 2350 | |||
SS14 2350 | |||
SS14 2350 | |||
SS14 2350 |
D 3758 (2003) | Seamless nickel-chromium-iron alloy pipes | D-3758-(2003).pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com