Korea KS D 3697 (2002), STS430WSB Specialsteel Stainless steel wires for cold heading and cold forging and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Type | Standard | Country | Application | 
|---|---|---|---|---|---|---|
| Steel Grades | Specialsteel | STS430WSB | Ferrite | KS | Korea | Stainless steel wires for cold heading and cold forging | 
| C | Si | Mn | P | S | Cr | Ni | Mo | N | 
|---|---|---|---|---|---|---|---|---|
| ≤0.12 | ≤0.75 | ≤1.00 | ≤0.040 | ≤0.030 | 16.00 -18.00 | ≤0.60 | ≤ ≥ | ≤ ≥ | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 936 (≥) | 447 (≥) | 42 | 22 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 222 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 23 | - | - | 0.33 | - | |||
| 957 | 655 | - | 44.3 | 221 | - | ||
| 644 | - | 14 | 41.2 | 313 | 132 | 
Heat treated : 1918°C - 1236°C
| D 3697 (2002) | Stainless steel wires for cold heading and cold forging | D-3697-(2002).pdf | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com