Korea KS D 3690 (2009), STS316LCA Specialsteel Cold - rolled formed stainless steel equal leg angles and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | STS316LCA | Austenite | KS | Korea | Cold - rolled formed stainless steel equal leg angles |
C | Si | Mn | P | S | Cr | Ni | Mo | N |
---|---|---|---|---|---|---|---|---|
≤0.03 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.030 | 16.00 -18.00 | 12.00 -15.00 | 2.00 -3.00 | ≤ ≥ |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
278 (≥) | 862 (≥) | 31 | 21 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 344 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
43 | - | - | 0.32 | - | |||
511 | 517 | - | 21.3 | 412 | - | ||
131 | - | 23 | 23.2 | 224 | 411 |
Heat treated : 1499°C - 1264°C
D 3690 (2009) | Cold - rolled formed stainless steel equal leg angles | D-3690-(2009).pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com