Korea KS D 3692 (2001), D 3702 (2008), D 3703 (2007), D 3706 (2008), STS316F Specialsteel Stainless steel bars and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Type | Standard | Country | Application | 
|---|---|---|---|---|---|---|
| Steel Grades | Specialsteel | STS316F | Austenite | KS | Korea | Stainless steel bars | 
| C | Si | Mn | P | S | Cr | Ni | Mo | N | 
|---|---|---|---|---|---|---|---|---|
| ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.030 | 16.00 -18.00 | 10.00 -14.00 | 2.00 -3.00 | ≤ ≥ | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 333 (≥) | 188 (≥) | 21 | 23 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 124 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 33 | - | - | 0.32 | - | |||
| 111 | 561 | - | 34.3 | 142 | - | ||
| 367 | - | 23 | 41.2 | 243 | 412 | 
Heat treated : 1684°C - 1957°C
| D 3692 (2001) | Cold finished stainless steel bars | D-3692-(2001).pdf | 
| D 3702 (2008) | Stainless steel wire rods | D-3702-(2008).pdf | 
| D 3703 (2007) | Stainless steel wires | D-3703-(2007).pdf | 
| D 3706 (2008) | Stainless steel bars | D-3706-(2008).pdf | 