France AFNOR NF A 35-578, Z6CND17-13B Specialsteel Iron and steel. Stainless steel for high temperature application and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Specialsteel | Z6CND17-13B | AFNOR | France | Iron and steel. Stainless steel for high temperature application |
C | Si | Mn | P | S | Cr | Mo | Ni | B |
---|---|---|---|---|---|---|---|---|
0.04 -0.08 | ≤0.75 | ≤2.00 | ≤0.040 | ≤0.015 | 16.00 -18.00 | 12.00 -14.00 | 2.00 -2.50 | 0.0015 -0.0060 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
179 (≥) | 886 (≥) | 43 | 13 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 431 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
11 | - | - | 0.34 | - | |||
966 | 481 | - | 34.3 | 111 | - | ||
689 | - | 32 | 44.2 | 442 | 313 |
Heat treated : 1699°C - 1612°C
Grade | Standard | Country | Application |
---|---|---|---|
Z6CND17-13B |
NF A 35-578 | Iron and steel. Stainless steel for high temperature application | NF-A-35-578.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...