USA AISI S30415 Specialsteel Stainless steel and heat resistant steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | S30415 | Austenite | AISI | USA | Stainless steel and heat resistant steel |
C | Si | Mn | P | S | Cr | Ni | N | Ce |
---|---|---|---|---|---|---|---|---|
0.04 -0.06 | 1.00 -2.00 | ≤0.80 | ≤0.045 | ≤0.03 | 18.0 -19.0 | 9.00 -10.0 | 0.12 -0.18 | 0.03 -0.08 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
762 (≥) | 637 (≥) | 32 | 14 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 233 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
13 | - | - | 0.13 | - | |||
794 | 879 | - | 42.3 | 224 | - | ||
794 | - | 33 | 41.2 | 331 | 432 |
Heat treated : 1956°C - 1342°C
Grade | Standard | Country | Application |
---|---|---|---|
304H | |||
304HN | |||
304HN | |||
304H | |||
TP304H | |||
TP304H | |||
TP304H | |||
SUS304HFB | |||
SUS304HTP | |||
SUS304HTB | |||
SUS304HTB | |||
SUS304HTP | |||
SUS304HFB | |||
304HN(S30452) | |||
SUS304HFB | |||
SUS304HFB | |||
SUS304HTP | |||
SUS304HTP |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...