France AFNOR NF A 35-577, Z6CND17-11-02FF Specialsteel Iron and steel. Stainless steel wire rods for cold forming and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Specialsteel | Z6CND17-11-02FF | AFNOR | France | Iron and steel. Stainless steel wire rods for cold forming |
C | Si | Mn | P | S | Cr | Mo | Ni |
---|---|---|---|---|---|---|---|
0.040 -0.070 | 0.50 -1.00 | 1.00 -1.50 | ≤0.040 | ≤0.010 | 16.50 -17.50 | 2.00 -2.50 | 10.50 -11.50 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
614 (≥) | 618 (≥) | 31 | 43 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 114 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
33 | - | - | 0.44 | - | |||
774 | 917 | - | 43.3 | 234 | - | ||
784 | - | 33 | 42.2 | 242 | 442 |
Heat treated : 1468°C - 1291°C
Grade | Standard | Country | Application |
---|---|---|---|
Z6CND17-11-02FF | |||
Z6CND17-11-02FF |
NF A 35-577 | Iron and steel. Stainless steel wire rods for cold forming | NF-A-35-577.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com