France AFNOR NF A 35-577, Z3CNU18-10FF Specialsteel Iron and steel. Stainless steel wire rods for cold forming and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Specialsteel | Z3CNU18-10FF | AFNOR | France | Iron and steel. Stainless steel wire rods for cold forming |
| C | Si | Mn | P | S | Cr | Mo | Ni | Cu |
|---|---|---|---|---|---|---|---|---|
| ≤0.030 | ≤0.75 | ≤2.00 | ≤0.040 | 0.015 -0.030 | 17.00 -19.00 | ≤ ≥ | 9.00 -10.00 | 3.00 -3.50 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 944 (≥) | 746 (≥) | 43 | 33 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 243 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 23 | - | - | 0.34 | - | |||
| 758 | 448 | - | 22.3 | 144 | - | ||
| 191 | - | 21 | 44.2 | 241 | 211 |
Heat treated : 1333°C - 1882°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| Z3CNU18-10 | |||
| Z3CNU18-10 | |||
| Z3CNU18-10FF | |||
| Z3CNU18-10FF |
| NF A 35-577 | Iron and steel. Stainless steel wire rods for cold forming | NF-A-35-577.pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com