Japan JIS G 4308 (2007), SUS 303 Specialsteel Stainless steel wire rods and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Type | Standard | Country | Application | 
|---|---|---|---|---|---|---|
| Steel Grades | Specialsteel | SUS 303 | Austenite | JIS | Japan | Stainless steel wire rods | 
| C | Si | Mn | P | S | Cr | Ni | Mo | N | 
|---|---|---|---|---|---|---|---|---|
| ≤0.15 | ≤1.00 | ≤2.00 | ≤0.20 | ≤0.15 | 17.00 -19.00 | 8.00 -10.00 | ≤0.60 | ≤ ≥ | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 645 (≥) | 758 (≥) | 23 | 41 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 412 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.42 | - | |||
| 236 | 598 | - | 44.3 | 332 | - | ||
| 974 | - | 42 | 41.2 | 112 | 322 | 
Heat treated : 1667°C - 1169°C
| G 4308 (2007) | Stainless steel wire rods | G-4308-(2007).pdf | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com