Japan JIS G 4308 (2007), SUS 303 Cu Specialsteel Stainless steel wire rods and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Type | Standard | Country | Application | 
|---|---|---|---|---|---|---|
| Steel Grades | Specialsteel | SUS 303 Cu | Austenite | JIS | Japan | Stainless steel wire rods | 
| C | Si | Mn | P | S | Cr | Ni | Mo | N | Cu | 
|---|---|---|---|---|---|---|---|---|---|
| ≤0.15 | ≤1.00 | ≤3.00 | ≤0.20 | ≤0.15 | 17.00 -19.00 | 8.00 -10.00 | ≤0.60 | ≤ ≥ | 1.50 -3.50 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 541 (≥) | 792 (≥) | 13 | 12 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 43 | - | - | 0.22 | - | |||
| 734 | 537 | - | 22.3 | 434 | - | ||
| 964 | - | 32 | 14.2 | 322 | 332 | 
Heat treated : 1241°C - 1925°C
| G 4308 (2007) | Stainless steel wire rods | G-4308-(2007).pdf | 