Japan JIS G 4317 (2005), SUS 304N2 Specialsteel Hot-formed stainless steel sections and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | SUS 304N2 | Austenite | JIS | Japan | Hot-formed stainless steel sections |
C | Si | Mn | P | S | Cr | Ni | Mo | N |
---|---|---|---|---|---|---|---|---|
≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 18.00 -20.00 | 8.00 -10.50 | ≤ ≥ | ≤ ≥ |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
262 (≥) | 165 (≥) | 43 | 23 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.22 | - | |||
996 | 153 | - | 41.3 | 422 | - | ||
714 | - | 21 | 33.2 | 332 | 244 |
Heat treated : 1422°C - 1829°C