Japan JIS G 4317 (2005), SUS 347 Specialsteel Hot-formed stainless steel sections and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | SUS 347 | Austenite | JIS | Japan | Hot-formed stainless steel sections |
C | Si | Mn | P | S | Cr | Ni | Mo | N | Nb |
---|---|---|---|---|---|---|---|---|---|
≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 17.00 -19.00 | 9.00 -13.00 | ≤ ≥ | ≤ ≥ | 10×C% - ≥ |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
973 (≥) | 911 (≥) | 21 | 21 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 234 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
31 | - | - | 0.13 | - | |||
227 | 823 | - | 41.3 | 344 | - | ||
168 | - | 23 | 13.2 | 344 | 214 |
Heat treated : 1176°C - 1959°C
G 4317 (2005) | Hot-formed stainless steel sections | G-4317-(2005).pdf |