USA SAE SAE J 470 (1976), UNITEMP 750 Specialsteel Wrought nickel and nickel-related alloys and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | UNITEMP 750 | Precipitation-Hardening | SAE | USA | Wrought nickel and nickel-related alloys |
C | Si | Mn | Cr | Ni | Mo | Co | W | Al | Cu | Ti | Fe | Nb | B |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
≤0.04 | ≤ ≥ | ≤ ≥ | ≤15.50 | ≤remaining | ≤ ≥ | ≤ ≥ | ≤ ≥ | ≤1.20 | ≤ ≥ | ≤2.30 | ≤7.00 | ≤1.00 | ≤0.003 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
991 (≥) | 329 (≥) | 41 | 43 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 424 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
23 | - | - | 0.43 | - | |||
886 | 721 | - | 12.3 | 142 | - | ||
847 | - | 43 | 44.2 | 223 | 432 |
Heat treated : 1694°C - 1924°C
SAE J 470 (1976) | Wrought nickel and nickel-related alloys | SAE-J-470-(1976).pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...