USA SAE B 622 (2010), B 622 R20033 Specialsteel Seamless Nickel and Nickel-Cobalt Alloy Pipe and Tube and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | B 622 R20033 | Precipitation-Hardening | SAE | USA | Seamless Nickel and Nickel-Cobalt Alloy Pipe and Tube |
C | Si | Mn | Cr | Ni | Mo | Co | W | Al | Cu | Ti | Fe | Nb |
---|---|---|---|---|---|---|---|---|---|---|---|---|
≤0.12 | ≤0.30 | ≤0.80 | ≤19.00 | ≤14.00 | ≤ ≥ | ≤ ≥ | ≤ ≥ | ≤ ≥ | ≤ ≥ | ≤ ≥ | ≤remaining | ≤1.60 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
547 (≥) | 827 (≥) | 13 | 11 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 143 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
43 | - | - | 0.33 | - | |||
199 | 667 | - | 14.3 | 432 | - | ||
515 | - | 14 | 33.2 | 123 | 433 |
Heat treated : 1271°C - 1847°C
Grade | Standard | Country | Application |
---|---|---|---|
R-20 | |||
25Cr-20Ni | |||
25Cr-20Ni+ | |||
29Cr-20Ni | |||
25Cr-20Ni | |||
25Cr-20Ni | |||
25Cr-20Ni | |||
25Cr-20Ni | |||
25Cr-20Ni | |||
29Cr-20Ni | |||
29Cr-20Ni | |||
29Cr-20Ni |
B 622 (2010) | Seamless Nickel and Nickel-Cobalt Alloy Pipe and Tube | B-622-(2010).pdf |