USA AISI S30200 Specialsteel Austenitic Chromium Nickel Stainless Steel and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Class | Grade | Type | Standard | Country | Application | 
|---|---|---|---|---|---|---|
| Steel Grades | Specialsteel | S30200 | Austenite | AISI | USA | Austenitic Chromium Nickel Stainless Steel | 
| C | Si | Mn | P | S | Cr | Ni | 
|---|---|---|---|---|---|---|
| ≤0.15 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.03 | 16.0 -18.0 | 6.00 -8.00 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 242 (≥) | 275 (≥) | 34 | 23 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 233 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 42 | - | - | 0.11 | - | |||
| 258 | 522 | - | 21.3 | 214 | - | ||
| 125 | - | 41 | 22.2 | 441 | 233 | 
Heat treated : 1695°C - 1355°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| 1.4301 | |||
| 1.4301 | |||
| 1.4301 | |||
| 1.4301 | |||
| 1.4301 | |||
| 1.0301 | |||
| 301 | |||
| S30100 | |||
| 301L | |||
| S30103 | |||
| 301LN | |||
| S30153 | |||
| R30155 | |||
| S63016 | |||
| S63017 | |||
| S63014 | |||
| S63015 | |||
| S63011 | |||
| S63012 | |||
| S63013 | 
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com