USA SAE A 959 (2011), A 959 S32950 Specialsteel Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels and Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Class | Grade | Type | Standard | Country | Application |
---|---|---|---|---|---|---|
Steel Grades | Specialsteel | A 959 S32950 | Duplex steel | SAE | USA | Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels |
C | Mn | Si | P | S | Cr | Ni | Mo | N |
---|---|---|---|---|---|---|---|---|
≤0.03 | ≤2.00 | ≤0.60 | ≤0.035 | ≤0.01 | 26.00 -29.00 | 3.50 -5.20 | 1.00 -2.50 | 0.15 -0.25 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
712 (≥) | 726 (≥) | 41 | 12 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 211 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
32 | - | - | 0.34 | - | |||
896 | 871 | - | 32.3 | 331 | - | ||
229 | - | 42 | 24.2 | 234 | 113 |
Heat treated : 1644°C - 1699°C
Grade | Standard | Country | Application |
---|---|---|---|
7-MoPLUS | |||
S32950 | |||
S32950 | |||
7-Mo PLUS(S32950) | |||
S32950 |
A 959 (2011) | Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels | A-959-(2011).pdf |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com